It is a preventive maintenance procedure to stabilize the surface of the existing oxidized asphalt surface which is on verge of developing raveling (loss of fines from the matrix). It consists of applying diluted Slow setting (SS) emulsion with a bitumen distributor.
It is a preventive maintenance procedure to stabilize the surface of the existing oxidized asphalt surface which is on verge of developing raveling (loss of fines from the matrix). It consists of applying diluted Slow setting (SS) emulsion with a bitumen distributor.